Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 35.0 - 221 MPa | 5080 - 32000 psi | Average value: 112 MPa Grade Count:10 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Compressive Yield Strength | 35.0 MPa | 5080 psi | ASTM D395 |
Covestro Baydur® GS-772 Polyurethane Solid RIM, MDI-based 2-Component Liquid System 0.25 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Compressive Yield Strength | 35.0 - 160 MPa @Temperature 120 - 250 °C |
5080 - 23200 psi @Temperature 248 - 482 °F |
Average value: 101 MPa Grade Count:9 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |
|||
Compressive Yield Strength | 35.0 - 285 MPa | 5080 - 41300 psi | Average value: 235 MPa Grade Count:29 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |