Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 142 MPa | 20600 psi | DIN EN ISO 604 |
Wolf Kunststoff ZEDEX® ZX-410 A4A Polymer Alloy ZX-410 is a bearing material with excellent properties and a very affordable price.Main Characteristics: Hard, Stiff, Tough; High dimensional stability; High chemical resistance; High water resistan.. |
|||
Compressive Yield Strength | 142 MPa | 20600 psi | 10% Strain; EN ISO 604 |
Ensinger TECASINT™ 2061 Polyimide, 15% Graphite, 10% PTFE Filled (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |
|||
Compressive Yield Strength | 142 - 250 MPa | 20600 - 36300 psi | Average value: 194 MPa Grade Count:22 |
Overview of materials for Melamine-Phenolic Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap.. |