Mechanical Properties Metric English Comments
Compressive Yield Strength 2.76 - 1690 MPa
400 - 246000 psi
Average value: 358 MPa Grade Count:79
Overview of materials for Epoxy Cure Resin
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M..
Compressive Yield Strength 2.76 MPa
400 psi
Stabilized, typ
Hexcel® HexWeb® HRH-10/F50 - 3.5 Nonmetallic Flex-Core Honeycomb
Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo..
Compressive Yield Strength >= 2.76 MPa
>= 400 psi
Stabilized, min
Hexcel® HexWeb® HRH-327 - 3/16 - 4.5 Fiberglass Reinforced Polyimide Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a..
Compressive Yield Strength >= 2.76 MPa
>= 400 psi
Stabilized, min
Hexcel® HexWeb® HRP - 1/4 - 3.5 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Compressive Yield Strength >= 2.76 MPa
>= 400 psi
Bare, min
Hexcel® HexWeb® HRP - 3/16 - 4.0 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Compressive Yield Strength 2.76 MPa
400 psi
Stabilized, typ
Hexcel® HexWeb® HRP/F35 - 3.5 Nonmetallic Flex-Core Honeycomb
Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo..
Compressive Yield Strength 2.76 MPa
400 psi
Bare, typ
Hexcel® HexWeb® CR III 1/4-5056-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Compressive Yield Strength 2.76 MPa
400 psi
Bare, typ
Hexcel® HexWeb® CR-PAA™ 1/4-5056-0.0015 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Compressive Yield Strength >= 2.76 MPa
>= 400 psi
Bare, min
Hexcel® HexWeb® HRH-10 - 1/8- 4.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Compressive Yield Strength 2.76 MPa
400 psi
TM R050-38
Resinlab® EP1200LV Casting Resin
Resinlab™ EP1200LV a low viscosity version of EP1200, a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity, flexibility an..