Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 18.0 MPa | 2610 psi | at 5% nominal strain; ISO 604 |
Quadrant EPP Cestilene™ HD 1000 R Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Compressive Yield Strength | 18.0 - 86.2 MPa | 2610 - 12500 psi | Average value: 60.4 MPa Grade Count:6 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Compressive Yield Strength | 18.0 MPa | 2610 psi | |
Sawbones Solid Rigid Polyurethane Foam 30 pcf Density Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mech.. |