Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Sawbones Solid Rigid Polyurethane Foam 30 pcf Density

Category Other Engineering Material , Composite Core Material , Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane Foam, Unreinforced
Manufacturer Sawbones
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sawbones Solid Rigid Polyurethane Foam 30 pcf Density.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mechanical properties of human bone, however, it does provide consistent and uniform material with properties in the range of human cancellous bone. Relevant mechanical properties for comparison to human cancellous bone may depend on the particular test method that is being developed.The ASTM F-1839-08 "Standard Specification for Rigid Polyurethane Foam for Use as a Standard Material for Testing Orthopaedic Devices and Instruments" states that, "The uniformity and consistent properties of rigid polyurethane foam make it an ideal material for comparative testing of bones screws and other medical devices and instruments."DescriptionSolid rigid polyurethane foam has a closed cell content ranging from 96.0 to 99.9%. Foam is available in a range of sizes and densities, from 0.08 to 0.80 grams per cubic centimeter (5 to 50 pounds per cubic foot).. Standard block size: 13cm X 18cm X 4cm Standard sheet size: 13cm X 18cm X 3mm Other NotesWater absorption ranges from 0.301 to 0.0 kg/m2Foam meets ASTM F-1839-08. Block dimensions are within ±2mm and sheet thickness is within ±0.3mm. Foam density may vary ±10%. Properties parallel to direction of the rise of foam. Information provided by Sawbones.
Physical Properties Metric English Comments
Density 0.480 g/cc
0.0173 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength 12.0 MPa
1740 psi
Tensile Modulus 0.592 GPa
85.9 ksi
Compressive Yield Strength 18.0 MPa
2610 psi
Compressive Modulus 0.445 GPa
64.5 ksi
Poissons Ratio 0.30
0.30
Shear Modulus 0.870 GPa
126 ksi
Shear Strength 7.60 MPa
1100 psi
Thermal Properties Metric English Comments
CTE, linear 63.0 µm/m-°C

@Temperature -46.0 - 93.0 °C
35.0 µin/in-°F

@Temperature -50.8 - 199 °F
Users viewing this material also viewed the following: