Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Yield Strength = 142 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 142 MPa
20600 psi
DIN EN ISO 604
Wolf Kunststoff ZEDEX® ZX-410 A4A Polymer Alloy
ZX-410 is a bearing material with excellent properties and a very affordable price.Main Characteristics: Hard, Stiff, Tough; High dimensional stability; High chemical resistance; High water resistan..
Compressive Yield Strength 142 MPa
20600 psi
10% Strain; EN ISO 604
Ensinger TECASINT™ 2061 Polyimide, 15% Graphite, 10% PTFE Filled (PI)
TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications...
Compressive Yield Strength 142 - 250 MPa
20600 - 36300 psi
Average value: 194 MPa Grade Count:22
Overview of materials for Melamine-Phenolic Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap..