Polymer Property : Compressive Yield Strength = 0.655 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 0.655 MPa
95.0 psi
Stabilized, typ
Hexcel® HexWeb® CR III 3/8-5052-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Compressive Yield Strength >= 0.655 MPa
>= 95.0 psi
Stabilized, min
Hexcel® HexWeb® HRH-10/OX - 3/16 - 1.8 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Compressive Yield Strength 0.655 MPa
95.0 psi
Stabilized
Hexcel® HexWeb® HRH-78 - 3/8 - 1.5 Commercial Grade Nomex Honeycomb/Phenolic Resin
Designation: Material-Cell Size (inches)-DensityHexWeb HRH-78 is manufactured from commercial grade aramid paper sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after..
Compressive Yield Strength 0.655 MPa
95.0 psi
Stabilized, typ
Hexcel® HexWeb® CR-PAA™ 3/8-5052-0.001 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Compressive Yield Strength >= 0.655 MPa
>= 95.0 psi
Stabilized, min
Hexcel® HexWeb® HRH-10 - 1/2 - 2.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Compressive Yield Strength >= 0.655 MPa
>= 95.0 psi
Stabilized, min
Hexcel® HexWeb® HRH-10 - 1/8- 1.8 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Compressive Yield Strength >= 0.655 MPa
>= 95.0 psi
Bare, min
Hexcel® HexWeb® HRH-10 - 3/16 - 1.8 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Compressive Yield Strength 0.655 MPa
95.0 psi
Bare, typ
Hexcel® HexWeb® HRH-10 - 3/8 - 1.5 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..