Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Graves Tear Strength | 88.0 kN/m @Thickness 0.760 mm |
502 pli @Thickness 0.0299 in |
on extruded sheet; ASTM D624 |
BASF Elastollan® 1185A10W Wire & Cable Grade Polyurethane Elastomer As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Graves Tear Strength | 88.0 kN/m @Thickness 0.762 mm |
502 pli @Thickness 0.0300 in |
extruded sheet; ASTM D624 |
BASF Elastollan® 1185A10X Wire & Cable Grade Polyurethane Elastomer Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Graves Tear Strength | 88.0 kN/m @Thickness 0.762 mm |
502 pli @Thickness 0.0300 in |
extruded sheet; ASTM D624 |
BASF Elastollan® 1185A10U Wire & Cable Grade Polyurethane Elastomer As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Graves Tear Strength | 88.0 kN/m @Thickness 0.762 mm |
502 pli @Thickness 0.0300 in |
extruded sheet; ASTM D624 |
BASF Elastollan® 1185A10V Wire & Cable Grade Polyurethane Elastomer Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Graves Tear Strength | 88.0 kN/m @Thickness 0.760 mm |
502 pli @Thickness 0.0299 in |
on extruded sheet; ASTM D624 |
BASF Elastollan® 1185A10Y Wire & Cable Grade Polyurethane Elastomer Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |