Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 45.0 - 60.0 MPa | 6530 - 8700 psi | ASTM D790-03 |
Proto3000 Objet Digital Materials™ DM_8425 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide.. |
|||
Flexural Strength | 45.0 - 60.0 MPa | 6530 - 8700 psi | ASTM D790-03 |
Proto3000 Objet Digital Materials™ DM_8505Gray50 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |
|||
Flexural Strength | 35.0 - 60.0 MPa | 5080 - 8700 psi | Transverse |
Quadrant Plastic Composites MultiQ® Concrete Thermoplastic Panel Composite MultiQ is a product line of thermoplastic composites in panel form whose specific properties make them particularly suitable as an environmental alternative to plywood in outdoor applications. Howev.. |
|||
Flexural Strength | 50.0 - 60.0 MPa | 7250 - 8700 psi | ISO 178 |
Raschig Group EN 5004 Epoxy Molding Compound Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo.. |
|||
Flexural Strength | 50.0 - 60.0 MPa | 7250 - 8700 psi | ISO 178 |
Raschig Group EN 5007 Epoxy Molding Compound Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo.. |
|||
Flexural Strength | 30.0 - 60.0 MPa | 4350 - 8700 psi | ASTM D790 |
Raschig Group PiMC 1221 High gloss PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Flexural Strength | 30.0 - 60.0 MPa | 4350 - 8700 psi | ASTM D790 |
Raschig Group PiMC 1241 Sanitary, uni color PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Flexural Strength | 30.0 - 60.0 MPa | 4350 - 8700 psi | ASTM D790 |
Raschig Group PiMC 1249 Sanitary, mix color PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |
|||
Flexural Strength | 30.0 - 60.0 MPa | 4350 - 8700 psi | ASTM D790 |
Raschig Group PiMC 1949 Granite colors PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa.. |