Mechanical Properties Metric English Comments
Flexural Strength 58.8 MPa
8530 psi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Infino® XI-2008F PPS/PPA, Mineral Filled
Information provided by Samsung Cheil Industries.
Flexural Strength 58.8 MPa
8530 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® AS-0151BS ABS, Unreinforced
Anti-static material that can be used in the housing of OA devices, IC, LSI carrier etc.Information provided by Samsung Cheil Industries.
Flexural Strength 58.8 MPa
8530 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® HF-0660I ABS, Unreinforced
Material with high flowability and high stiffness that can be used for vacuum cleaner, telephone, TV, VCR, calculator, radio and air-conditionerInformation provided by Samsung Cheil Industries.
Flexural Strength 58.8 MPa
8530 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® HF-0660IW ABS, Unreinforced
WNP high flow ABS materialInformation provided by Samsung Cheil Industries.
Flexural Strength 58.8 MPa
8530 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® SD-0150UF ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Flexural Strength 58.8 MPa
8530 psi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Starex® TX-0520 TRABS, Unreinforced
Information provided by Samsung Cheil Industries.
Flexural Strength 58.8 MPa
8530 psi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Starex® TX-0520T TRABS, Unreinforced
Information provided by Samsung Cheil Industries.
Flexural Strength 58.8 MPa
8530 psi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Starex® WR-9100 ASA, Unreinforced
Information provided by Samsung Cheil Industries.
Flexural Strength 58.8 MPa
8530 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® AS-0151BS ABS, Unreinforced
Anti-static material that can be used in the housing of OA devices, IC, LSI carrier etc.Information provided by Samsung Cheil Industries.
Flexural Strength 58.8 MPa
8530 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® HF-0660I ABS, Unreinforced
Material with high flowability and high stiffness that can be used for vacuum cleaner, telephone, TV, VCR, calculator, radio and air-conditionerInformation provided by Samsung Cheil Industries.
Flexural Strength 58.8 MPa
8530 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® HF-0660IW ABS, Unreinforced
WNP high flow ABS materialInformation provided by Samsung Cheil Industries.
Flexural Strength 58.8 MPa
8530 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® SD-0150UF ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Flexural Strength 58.8 MPa
8530 psi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Starex® TX-0520 TRABS, Unreinforced
Information provided by Samsung Cheil Industries.
Flexural Strength 58.8 MPa
8530 psi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Starex® TX-0520T TRABS, Unreinforced
Information provided by Samsung Cheil Industries.
Flexural Strength 58.8 MPa
8530 psi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Starex® VS-0826 ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Flexural Strength 58.8 MPa
8530 psi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Starex® WR-9100 ASA, Unreinforced
Information provided by Samsung Cheil Industries.
Flexural Strength 58.8 MPa
8530 psi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Starex® WR-9310 ASA, Unreinforced Heat Resistant
Heat resistant ASA that is used in the interior/exterior material of automobileInformation provided by Samsung Cheil Industries.
Flexural Strength 58.8 MPa

@Thickness 3.20 mm
8530 psi

@Thickness 0.126 in
ASTM D790
Supreme Petrochem SP 243 Toughened Polystyrene
CharacteristicsGood flexibility Good clarity High stiffnessProcessing Extrusion ThermoformingApplications Clear thermoformed containers Oriented PS films LidsMaterial Status: Commercial : ActiveA..
Flexural Strength 58.8 MPa

@Thickness 3.20 mm
8530 psi

@Thickness 0.126 in
ASTM D790
Supreme Petrochem SP 253 Toughened Polystyrene
Characteristics High rigidity Improved toughness Good clarityProcessing Injection moldingApplications Ball pens Small appliances housings Small impellersMaterial Status: Commercial : ActiveAgenc..
Flexural Strength 58.8 MPa

@Thickness 3.20 mm
8530 psi

@Thickness 0.126 in
ASTM D790
Supreme Petrochem SP 263 Toughened Polystyrene
CharacteristicsGood flexibility Easy flow Good stiffnessProcessing Injection moldingApplications Transparent hangers Material Status: Commercial : ActiveAgency Ratings: FDA 21 CFR 177.1640Informatio..
Flexural Strength 58.8 MPa

@Thickness 3.20 mm
8530 psi

@Thickness 0.126 in
ASTM D790
Supreme Petrochem SP 6450 High Heat Polystyrene
Characteristics High impact and modulus Very good flow properties High heat resistance & strength Available in any dark colorProcessing Injection moldingApplications Instrument enclosures Automo..
Flexural Strength 58.8 MPa
8530 psi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Starex® WR-9310 ASA, Unreinforced Heat Resistant
Heat resistant ASA that is used in the interior/exterior material of automobileInformation provided by Samsung Cheil Industries.
Flexural Strength 58.8 MPa

@Temperature 260 °C
8530 psi

@Temperature 500 °F
ASTM D790
Daelim H&L Plavis-N CM Unfilled Aromatic Polyimide Bearing
Compression Molded. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS po..
Flexural Strength 58.8 MPa

@Temperature 260 °C
8530 psi

@Temperature 500 °F
ASTM D790
Daelim H&L Plavis-N ISO Unfilled Aromatic Polyimide Bearing
Isostatically Molded. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS ..
Flexural Strength 58.8 MPa
8530 psi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Starex® VS-0826 ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Flexural Strength 58.8 MPa
8530 psi
2.8 mm/min; ASTM D638
Samsung Cheil Industries Infino® XI-2008F PPS/PPA, Mineral Filled
Information provided by Samsung Cheil Industries.
Copyright © lookpolymers.com All Rights Reserved