Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 55.8 MPa | 8090 psi | ASTM D790 |
PolyOne Maxxam™ PD 40 TF Black Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Strength | 55.8 MPa | 8090 psi | |
Poco Graphite EDM-200 EDM Graphite POCO's EDM-200 is an isotropic Superfine particle graphite providing good strength, surface finish, and wear resistance.Applications:Structural ribsRoughing or finishing electrodesLarge featured mol.. |
|||
Flexural Strength | 55.8 MPa @Temperature 175 °C |
8090 psi @Temperature 347 °F |
4; ISO 178 |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention.. |
|||
Flexural Strength | 55.8 MPa | 8090 psi | ASTM D790 |
Eastman Tenite 360A4861307 Cellulose Acetate Propionate, Clear, Trsp Applications:Blood TherapyDrug DeliveryIV ComponentsMedical DevicesSurgical InstrumentsKey Attributes:Chemical resistance to most medical solvents including lipids and IPAEase of processingGamma and.. |
|||
Flexural Strength | 55.8 MPa @Temperature 175 °C |
8090 psi @Temperature 347 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of .. |