Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 37.93 MPa
5501 psi
ASTM D790
Lucent Polymers CPP-0107 Polypropylene Homopolymer
Recycled ContentAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Flexural Strength 37.93 MPa
5501 psi
ASTM D790
Lucent Polymers PPC-210 Polypropylene, Impact Modified
Add "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Flexural Strength 37.93 MPa
5501 psi
ASTM D790
Lucent Polymers PPC-220 Polypropylene, Impact Modified
Add "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Flexural Strength 37.93 MPa
5501 psi
ASTM D790
Lucent Polymers PPC-0222 Polypropylene, Impact Modified
Recycled ContentAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.