Mechanical Properties Metric English Comments
Flexural Strength 374 MPa
54200 psi
ASTM D790
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 (Asia Pacific)
LNP VERTON* RV00AES is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding.
Flexural Strength 374 MPa
54200 psi
ASTM D790
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 (Europe-Africa-Middle East)
LNP VERTON* RV00AES is a compound based on PA 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.
Flexural Strength 374 MPa
54200 psi
ASTM D790
SABIC Innovative Plastics LNP VERTON RV00AES PA 66
LNP VERTON* RV00AES is a compound based on Nylon 66 resin containing 50% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural.
Flexural Strength 374 MPa
54200 psi
ASTM D790
SABIC Innovative Plastics LNP VERTON RX06422 PA 66
LNP VERTON* RX06422 is a compound based on Nylon 66 resin containing 50% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural.
Flexural Strength 374 MPa
54200 psi
ASTM D790
SABIC Innovative Plastics LNP VERTON RX06422 PA 66 (Asia Pacific)
LNP VERTON* RX06422 is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding.