Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 1720 MPa | 249000 psi | |
CoorsTek ACI-Ni6 Tungsten Carbide Applications: seal rings, plungers, liners, nozzles, valve components, pump components, wear components in the oil & gas, construction, and agriculture equipment industries |
|||
Flexural Strength | 1720 MPa | 249000 psi | ASTM F417 |
CoorsTek YZTP Yttria Partially Stabilized Zirconia, Hipped Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Flexural Strength | 1720 MPa | 249000 psi | |
China Tungsten YG8C Cemented Tungsten Carbide for Mining Purposes For rotary rock drill bits for medium hard and hard rock; and for coal cutting picks and oil drill bits for cutting of honse-stone containing formations.Information provided by China Tungsten |
|||
Flexural Strength | 1720 MPa | 249000 psi | |
China Tungsten YG610 Tungsten Carbide Good thermal strength and high wear resistance .Continuous or intermittent cutting of cast irons, refractory alloys and quenched steelInformation provided by China Tungsten |