CoorsTek ACI-Ni6 Tungsten Carbide

Category Ceramic , Carbide
Manufacturer CoorsTek
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF CoorsTek ACI-Ni6 Tungsten Carbide.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications: seal rings, plungers, liners, nozzles, valve components, pump components, wear components in the oil & gas, construction, and agriculture equipment industries
Physical Properties Metric English Comments
Density 14.95 g/cc
0.5401 lb/in³
Particle Size 1.0 - 3.0 µm
1.0 - 3.0 µm
Grain Size
Mechanical Properties Metric English Comments
Hardness, Rockwell A 92
92
Modulus of Elasticity 607 GPa
88000 ksi
Flexural Strength 1720 MPa
249000 psi
Poissons Ratio 0.25
0.25
Shear Modulus 243 GPa
35200 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 5.20 µm/m-°C

@Temperature 25.0 - 400 °C
2.89 µin/in-°F

@Temperature 77.0 - 752 °F
5.80 µm/m-°C

@Temperature 25.0 - 800 °C
3.22 µin/in-°F

@Temperature 77.0 - 1470 °F
Specific Heat Capacity 0.210 J/g-°C
0.0502 BTU/lb-°F
Thermal Conductivity 82.0 W/m-K
569 BTU-in/hr-ft²-°F