Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 158 MPa | 22900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate.. |
|||
Flexural Strength | 158 MPa | 22900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate.. |
|||
Flexural Strength | 158 MPa | 22900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Internal mold release. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is halogen free.. |
|||
Flexural Strength | 158 MPa | 22900 psi | ASTM D790 |
PBI Performance Products Celazole® TL-60 Self Lubricating Melt Processable Polybenzimidazole Celazole® polybenzimidazole (PBI) resin is a unique and highly stable linear hetrocyclic polymer. PBI is characterized by high strength; excellent thermal stability, and broad chemical resistance. .. |
|||
Flexural Strength | 158 MPa | 22900 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL14 PC LNP LUBRICOMP* DFL14 is a compound based on Polycarbonate resin containing 20% Glass Fiber and 5% PTFE. Added features include: Internally Lubricated. |
|||
Flexural Strength | 158 MPa | 22900 psi | 50.8 mm Span, 1 mm/min; ASTM D790 |
LNP NORYL® EXCP0112 PPS + Polyphenylene Ether, 40% Glass / Mineral Reinforcement
(discontinued **) For applications requiring voltage resistance.Features: Corona resistantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labele.. |
|||
Flexural Strength | <= 158 MPa | <= 22900 psi | ISO 178 |
Polykemi AB POLYfill PPH GF8030 HC Polypropylene Homopolymer, Glass Fibre-Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 158 MPa | 22900 psi | ASTM D790 |
Idemitsu Kosan Xarec® N WA 7010 SPS, 10% Glass Filled
(discontinued **) Crystalline Polymer Blend, Glass Filled. Used in Automotive Electronics applications. |
|||
Flexural Strength | 158 MPa @Temperature 22.0 °C |
22900 psi @Temperature 71.6 °F |
25 mm wide 100 mm long, flat samples; ISO 14125 |
Menzolit Menzolit® SMC 0190 Unsaturated Polyester UP SMC 0190 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Flexural Strength | 158 MPa | 22900 psi | ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp RFM62 PA 66 (Asia Pacific) LNP* Lubricomp* RFM62 is a compound based on Nylon 66 resin containing Glass Fiber, Mineral.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Strength | 158 MPa | 22900 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT (Asia Pacific) LNP* Lubricomp* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Ret.. |
|||
Flexural Strength | 158 MPa | 22900 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DE0029 PC (Asia Pacific) LNP* Stat-kon* DE0029 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Flexural Strength | 158 MPa | 22900 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DX05474 PC LNP* STAT-KON* DX05474 is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Flame Retardant, Mold .. |
|||
Flexural Strength | 158 MPa | 22900 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DX05474 PC (Asia Pacific) LNP* Stat-kon* DX05474 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Flame Ret.. |
|||
Flexural Strength | 158 MPa | 22900 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON EX01696C PEI (Asia Pacific) LNP* Stat-kon* EX01696C is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System. |
|||
Flexural Strength | 158 MPa | 22900 psi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp GF008 PSU (Europe-Africa-Middle East) LNP* Thermocomp* GF008 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Strength | 158 MPa | 22900 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP JF003E PES (Asia Pacific) LNP* Thermocomp* JF003E is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
Flexural Strength | 158 MPa | 22900 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP QF004 PA 6/10 (Asia Pacific) LNP* Thermocomp* QF004 is a compound based on Nylon 6/10 resin containing Glass Fiber. |
|||
Flexural Strength | 158 MPa | 22900 psi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOTUF RF002I PA 66 LNP THERMOTUF* RF002I is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Flexural Strength | 158 MPa | 22900 psi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON MX02795 PP (Asia Pacific) LNP* Verton* MX02795 is a compound based on Polypropylene resin containing Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, UV Stabilized. |
|||
Flexural Strength | 158 MPa | 22900 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DEL329E PC LNP* Stat-kon* DEL329E is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Flame Retardant, Wear Resi.. |
|||
Flexural Strength | 158 MPa | 22900 psi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON MX02795 PP LNP* VERTON* MX02795 is a compound based on Polypropylene resin containing Proprietary Fillers. Added features of this material include: Heat Stabilized, UV Stabilized, Structural. |
|||
Flexural Strength | 158 MPa | 22900 psi | ASTM D790 |
SABIC Innovative Plastics NORYL CN5258 PPE+PS (Asia Pacific) 40% filled FR high modulus PPE/PS blend |
|||
Flexural Strength | 158 MPa | 22900 psi | ASTM D790 |
Diamond Polymers DIAMALOY 1001 CF20 20% Carbon Fiber Filled ABS Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Strength | 158 MPa | 22900 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DFP34 PC (Asia Pacific) LNP* Lubricomp* DFP34 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Flexural Strength | 158 MPa | 22900 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFP34 PC (Asia Pacific) LNP* Lubricomp* DFP34 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Flexural Strength | 158 MPa | 22900 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFP34 PC LNP* Lubricomp* DFP34 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Internally Lubricated. |