Polymer Property : Flexural Strength = 2200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 15.2 MPa
2200 psi
ASTM D790
Quadrant EPP Armor-X™ Non-Marring, Elastomer Polymeric Blend (ASTM Product Data Sheet)
Flexural Strength 15.2 MPa
2200 psi
ASTM D790
Quadrant EPP Fluorosint® 500 PTFE, synthetic mica-filled PTFE, compression molded (ASTM Product Data Sheet)
Flexural Strength 15.2 MPa
2200 psi
ASTM D790
Techmer ES HiFill® LDPE 0098 S LE
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforAdditive: Heat StabilizerFeatures: Low ExtractablesInformation provided by TP Composites, Inc.
Flexural Strength 15.2 MPa
2200 psi
ASTM-F417
CoorsTek PolyGlyde™ 3000 Self-Lubricating Seal
PolyGlyde seals offer low heat generation in high-friction and high-stress environments. These seals provide superior performance over traditional carbon materials: runs cooler – even in dry-runni..
Flexural Strength 15.2 MPa
2200 psi
ASTM D790
Quadrant EPP Semitron® ESd 500 HR PTFE, static dissipative, compression molded (ASTM Product Data Sheet)