Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
Plaskolite Optix® CA-75 General Purpose Acrylic Resin Injection Molding and Extrusion Grade Pellets. Highest heat resistance, medium flow. |
|||
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
Parker Chomerics PREMIER™ A220-ST EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
Polymer Resources NY66-EX1 High Viscosity Nylon 66 Nylon 66, High Viscosity (RV 220 to 260)Process: ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as .. |
|||
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
Polymer Resources PC/TP-GP2-G20 PC/Polyester Alloy, 20% Glass Reinforced Excellent Chemical Resistance, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p.. |
|||
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
Polymer Resources PPX-G15 Modified-PPO, 15% Glass Reinforced, High Flow Modified-Polyphenylene Oxide, 10% Glass Reinforced, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
PolyOne Geon™ 80520 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 121 MPa | 17500 psi | |
Poco Graphite EDM-4 EDM Graphite POCO's EDM-4 is our premier offering in the Ultrafine classification. This highly isotropic grade combines strength with moderate hardness, yielding superior electrode fabrication characteristics. T.. |
|||
Flexural Strength | 121 MPa | 17500 psi | 21% Glass Spray-up Laminate |
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica.. |
|||
Flexural Strength | 121 MPa | 17500 psi | |
Cookson Group Plaskon® 3200LS Mineral Filled Novolac Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.Exhibits exceptional reliability under very stringent testing. This material is designed to minimize stress on the encapsulated .. |
|||
Flexural Strength | 121 MPa | 17500 psi | |
Cookson Group Plaskon® ULS-12HLG Epoxy Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A state-of-the-art, ultra low stress epoxy encapsulant designed for packaging large, stress-sensitive DIPs, PLCCs and QFPs. It i.. |
|||
Flexural Strength | 121 MPa | 17500 psi | ISO 178 |
Premix Premi-Glas® 1265 VE 1265-VE (Compression Molded) Glass Reinforced Vinyl Ester TMC
(discontinued **)< Description: Premi-Glas® 1265 VE is a glass reinforced vinyl ester molding compound designed for automotive under the hood applications. Key features and benefits: Designed for Injection or Injecti.. |
|||
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
SABIC Innovative Plastics NORYL S100G20 PPE+PS (Asia Pacific) |
|||
Flexural Strength | 121 MPa | 17500 psi | ISO 178 |
Solvay Specialty Polymers KetaSpire® KT-XXXX Polyetheretherketone (PEEK) KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha.. |
|||
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
A. Schulman SCHULADUR® A GF10 10% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
A. Schulman SCHULADUR® A GF10 10% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Flexural Strength | 121 MPa | 17500 psi | 21% Glass Spray-up Laminate |
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica.. |
|||
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
A. Schulman SCHULADUR® A GF10 10% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Flexural Strength | 121 MPa | 17500 psi | |
Du-Co Ceramics DC-10-L-3 Steatite Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Flexural Strength | 121 MPa | 17500 psi | ASTM D790 |
Adell AJ-33 Nylon 66, 15% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Flexural Strength | 121 MPa @Temperature 100 °C |
17500 psi @Temperature 212 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® A-1240 L Polyphthalamide (PPA)
(discontinued **) Amodel A-1240 L is a 40% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten.. |