Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 94.5 MPa | 13700 psi | ASTM D790 |
PolyOne Geon™ Vinyl Cellular E2519 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Physical properties were measured on non-foamed profiles. Measured density of an extruded 1 thick free foamed part was 0.70 gms/cc at a 360 deg.F melt temperature.Information provided by PolyO.. |
|||
Flexural Strength | 94.5 MPa @Temperature 175 °C |
13700 psi @Temperature 347 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep .. |
|||
Flexural Strength | 94.5 MPa | 13700 psi | ASTM D790 |
Solvay Specialty Polymers Supradel® HTS-2401 High Temperature Sulfone Resin
(discontinued **) Supradel HTS-2401 is a high-temperature high-performance amorphous sulfone polymer designed for use in reinforced high temperature thermoplastic formulations. With its glass transition temperature o.. |
|||
Flexural Strength | 94.5 MPa @Temperature 175 °C |
13700 psi @Temperature 347 °F |
4; ISO 178 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr.. |
|||
Flexural Strength | 94.4 MPa | 13700 psi | chs 0.05 in/min; ASTM D790 |
Diamond Polymers NPP 60-8419G Clear Amorphous Polyester Copolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Strength | 94.8 MPa | 13700 psi | |
Abatron AboCast 8-3/Abocure 8-3 Epoxy 2-part solvent-free dielectric epoxy casting compound.Processing: 100/50 ratio (pbw); Gel time, 100 g (3.5 oz.): 265 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°C (212°F).. |
|||
Flexural Strength | 94.5 MPa | 13700 psi | ASTM D-790 |
Axiall ProTherm® 4345 Rigid PVC, Extrusion Georgia Gulf ProTherm® 4345 is a CPVC powder blend designed for extrusion applications requiring high heat deflection temperatures. Processing and stability along with overall physical properties .. |
|||
Flexural Strength | 94.5 MPa | 13700 psi | ASTM D790 |
PolyOne Geon™ CPVC LC500 Polyvinyl Chloride, Chlorinated (CPVC) Geon LC500 CPVC is an extrusion grade rigid compound. It is designed for applications where enhanced resistance at elevated temperatures is needed. LC500 demonstrates ease of processing with excelle.. |
|||
Flexural Strength | 94.5 MPa | 13700 psi | ASTM D790 |
Solvay Specialty Polymers Supradel® HTS-2400 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2400 is a high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and heat deflection temperature of 235°C, this resin extends the.. |