Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 77.2 MPa | 11200 psi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging 161J-1-3V/2188GC-3V Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 77.2 MPa | 11200 psi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging 2020 LO-TB Polyvinyl Chloride, Rigid (PVC, Rigid) Geon® 2020 LO-TB is a clear blue tint pellet compound designed for water bottle and other low odor appliations that require FDA sanctioned materials.Information provided by PolyOne |
|||
Flexural Strength | 77.2 MPa | 11200 psi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging 2188GC Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 77.2 MPa | 11200 psi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging 2188GC-1V Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 77.2 MPa | 11200 psi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging 2188GC-3V Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 77.2 MPa | 11200 psi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging 2188NT Polyvinyl Chloride, Rigid (PVC, Rigid) A transparent natural PVC bottle compound for blow molding applications.Information provided by PolyOne |
|||
Flexural Strength | 77.2 MPa | 11200 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion 87570 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Flexural Strength | 77.2 MPa | 11200 psi | ASTM D790 |
Plaskolite Vivak PETG Sheet VIVAK offers a balance of physical properties and ease of fabrication. It is ideally suited for complex parts requiring fabrication, including deep thermoforming draws and precise molded-in details... |
|||
Flexural Strength | 77.2 MPa | 11200 psi | ASTM D790 |
Niche Polymer ABSN3BK ABS Information provided by Niche Polymer |
|||
Flexural Strength | 77.2 MPa | 11200 psi | ASTM D790 |
PolyOne Lubri-Tech™ PS-15GB/15T Polybutylene Terephthalate (PBT), Glass Bead Filled, PTFE Lubricated
(discont Description/Features:Glass Bead FilledPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 77.2 MPa @Strain 1.23 % |
11200 psi @Strain 1.23 % |
|
Malvern Minerals Epoxy with 50% Novacite® Daper Quartz Filler Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo.. |
|||
Flexural Strength | 77.2 MPa | 11200 psi | ASTM D790 |
Chase Plastics CP Pryme® A100HH ABS Molding Resin, High Heat Information provided by Chase Plastics. |
|||
Flexural Strength | 77.2 MPa @Thickness 6.35 mm |
11200 psi @Thickness 0.250 in |
tangent; chs 2.5 in/min; 100 mm SL; ASTM D790 |
Diamond Polymers ABSPC 7430-1005T ABS/PC Injection Molding Grade Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Strength | 77.2 MPa | 11200 psi | ASTM D790 |
Ensinger XP-150 Compression Molded Polyimide Unfilled, Premium Grade The XP 150 Series are amorphous high performance polyimides with high permanent temperature and creep resistance, as well as excellent bearing and wear properties, and excellent long term thermal st.. |
|||
Flexural Strength | 77.2 MPa | 11200 psi | ASTM D-790 |
Axiall 7048A Rigid PVC, Extrusion Georgia Gulf 7048A is a general purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Impact Strength & ToughnessFlame RetardantColorabilityCert.. |
|||
Flexural Strength | 77.2 MPa | 11200 psi | ASTM D-790 |
Axiall 8264 Rigid PVC, Extrusion Georgia Gulf 8264 is a rigid PVC pellet compound suited for applications where transparency is important. 8264 is widely used for clear films, sheets, and profile shapes in the packaging industry. .. |
|||
Flexural Strength | 77.2 MPa @Thickness 3.20 mm |
11200 psi @Thickness 0.126 in |
1.3 mm/min, Injection Molded; ASTM D790 |
Styron EMERGE™ 9100 CR Polycarbonate (PC) / Polyethylene Terephthalate (PET) Overview: EMERGE™ PC/PET 9100 CR advanced resin is a polycarbonate blend with excellent chemical resistance. This grade was designed for use in medical equipment housings and can withstand repeated.. |