Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 75.8 MPa | 11000 psi | 1.3 mm/min; ASTM D790 |
PolyOne LubriOne™ ATH-000/04S Acetal (POM) Homopolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Polymer Resources TP-GP1-IM Polybutylene Terephthalate, Impact Modified, Medium Flow Polybutylene Terephthalate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
PolyOne Edgetek® AT-15GF/000 Acetal-Copolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
PolyOne Lubri-Tech™ AT-000/5T-2S Acetal-Copolymer, PTFE/Silicone Lubricated
(discontinued **) Description/Features:PTFE/Silicone LubricatedInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
LNP Lubricomp® GFL-4034 EM M Polysulfone, Milled Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **)& Features: Good Moldability, LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP g.. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® PCT1000 PC/PET Alloy PC/PET alloy with outstanding chemical resistance and impact strengthAll information provided by LTL Color Compounders, Inc. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | |
SGL Carbon Group EK 2200 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | |
SGL Carbon Group Ridurid® EK 60 High Performance Graphite Filled Plastic Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Techmer ES HiFill® PA12 Availability: North AmericaForms: PelletsFeatures: Low ViscosityTPCI# 8807105Information provided by TP Composites, Inc. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Techmer ES HiFill® PA12 L N MB Availability: North AmericaForms: PelletsFeatures: Low ViscosityTPCI# 8807105Information provided by TP Composites, Inc. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Techmer ES HiFill® PBT HS BK Availability: North AmericaForms: PelletsAdditive: Heat StabilizerFeatures: Good Flow, Good Processability and Heat StabilizedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Techmer ES HiFill FR® PA6 FR HS Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Techmer ES HiFill® PA12 E HS Availability: North AmericaForms: PelletsAdditive: Heat StabilizerFeatures: Heat StabilizedProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Total PSC 500 Polystyrene Polystyrene 500 is a high melt, easy flow crystal polystyrene for fast cycle injection molding. The high flow characteristics of this material make it easy to fill thin parts. 500 is utilized in pro.. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Chesterton MRS S2 Metal Rebuilding System An advanced ceramic composite for the resurfacing and protection of all metal surfaces. It is normally applied at a thickness of 250 microns (10 mils) per coat. Non-shrinking, 100% solids. MRS S2 is.. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D-790 |
Axiall CL-6400 Rigid PVC, Molding Georgia Gulf CL-6400 is a high flow clear PVC compound designed for thin wall parts and multi-cavity molds. It is ideally suited for a variety of electrical and appliance applications.Information p.. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Asahi Kasei Thermylene® P6-30FM-Y249B 30% Glass/Mineral Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D-790 |
Axiall 7555 Rigid PVC, Extrusion, White Georgia Gulf 7555 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: ToughnessDurabilityUL RatingChemical ResistanceEase of ProcessingIn.. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | ASTM D790 |
Chase Plastics CP Pryme® PCA300 General Purpose Polycarbonate/ABS Alloy (Utility Grade) Information provided by Chase Plastics. |
|||
Flexural Strength | 75.8 MPa | 11000 psi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® PCT2014 PC/PBT Alloy PC/PBT alloy with improved impact strengthAll information provided by LTL Color Compounders, Inc. |