Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 66.7 MPa | 9670 psi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WR-9120 ASA, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 66.7 MPa | 9670 psi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WX-9300 ASA, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 66.7 MPa | 9670 psi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WX-9300UV ASA, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 66.7 MPa | 9670 psi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WR-9120 ASA, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 66.7 MPa | 9670 psi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WX-9300 ASA, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 66.7 MPa | 9670 psi | 2.8 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WX-9300UV ASA, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 66.7 - 70.5 MPa | 9670 - 10200 psi | ASTM D790M |
DSM Somos® ProtoGen™ O-XT 18420 Epoxy Resin for Stereolithography, UV Postcure at HOC -2 DescriptionDSM Somos® ProtoGen O-XT 18420 is a liquid, ABS-like, photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demons.. |