Polymer Property : Flexural Strength = 6.00 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 6.00 MPa
870 psi
at 3.5% strain; ISO 178
FKuR Kunststoff Bio-Flex® F 1110 Compostable PLA Blend
The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta..
Flexural Strength 6.00 MPa
870 psi
SPS Guang Zhou POPTREEâ„¢ 6001 Flame-retarded Polyethylene
Characteristic: Low density, superior melt flow index, high notched impact strengthApplications: X'mas decorative productInformation Provided by SPS (Guang Zhou) Ltd.
Flexural Strength 6.00 MPa
870 psi
ASTM D 790
SABIC Innovative Plastics LNP Stat-kon TD000
LNP* Stat-kon* TD000 is a compound based on Polyurethane resin. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americas region.
Flexural Strength 6.00 MPa
870 psi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON TD000 PU
LNP* STAT-KON* TD000 is an unfilled compound based on Polyurethane resin. Added feature of this material is: Electrically Conductive.
Flexural Strength 6.00 MPa
870 psi
SAE J949
Azdel SuperLite® SL550600-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness)
AZDEL SuperLite® SL550600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Flexural Strength 6.00 MPa
870 psi
SAE J949
Azdel SuperLite® SL550700-100 PP Resin Matrix / 55% Glass Fiber (1 mm Molded Thickness)
AZDEL SuperLite® SL550700-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Flexural Strength 6.00 MPa
870 psi
SAE J949
Azdel SuperLite® SL550700-100 PP Resin Matrix / 55% Glass Fiber (3.5 mm Molded Thickness)
AZDEL SuperLite® SL550700-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Flexural Strength 6.00 MPa
870 psi
SAE J949
Azdel SuperLite® SL550900-100 PP Resin Matrix / 55% Glass Fiber (4 mm Molded Thickness)
AZDEL SuperLite® SL550900-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Flexural Strength 6.00 MPa
870 psi
SAE J949
Azdel SuperLite® SL551400-100 PP Resin Matrix / 55% Glass Fiber (5 mm Molded Thickness)
AZDEL SuperLite® SL551400-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Flexural Strength 6.00 MPa
870 psi
SAE J949
Azdel SuperLite® SL551000-100 PP Resin Matrix / 55% Glass Fiber (4.5 mm Molded Thickness)
AZDEL SuperLite® SL551000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Copyright © lookpolymers.com All Rights Reserved