Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 37.93 MPa | 5501 psi | ASTM D790 |
Lucent Polymers CPP-0107 Polypropylene Homopolymer Recycled ContentAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Strength | 37.93 MPa | 5501 psi | ASTM D790 |
Lucent Polymers PPC-210 Polypropylene, Impact Modified Add "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Strength | 37.93 MPa | 5501 psi | ASTM D790 |
Lucent Polymers PPC-220 Polypropylene, Impact Modified Add "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Strength | 37.93 MPa | 5501 psi | ASTM D790 |
Lucent Polymers PPC-0222 Polypropylene, Impact Modified Recycled ContentAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |