Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 361 MPa | 52400 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON REF42 PA 66 LNP* STAT-KON* REF42 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 361 MPa @Temperature -40.0 °C |
52400 psi @Temperature -40.0 °F |
ASTM Test |
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Conditioned) Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also.. |
|||
Flexural Strength | 361 MPa | 52400 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON REF42 PA 66 (Asia Pacific) LNP* Stat-kon* REF42 is a compound based on Nylon 66 resin containing Glass Fiber, Carbon Fiber. |