Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 32.4 MPa | 4700 psi | ASTM D790 |
Asahi Kasei Thermylene® P-10TC-1777 10% Talc Filled, UV Stabilized Polypropylene Information provided by Asahi Thermofil |
|||
Flexural Strength | 32.4 MPa | 4700 psi | ASTM D790 |
Adell RZ-16 Copolymer Polypropylene, 30% Calcium Carbonate Filled Data provided by Adell Plastics, Inc. |