Adell RZ-16 Copolymer Polypropylene, 30% Calcium Carbonate Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Calcium Carbonate (CaCO3) Filler
Manufacturer Adell Plastics, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adell RZ-16 Copolymer Polypropylene, 30% Calcium Carbonate Filled.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by Adell Plastics, Inc.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Water Absorption 0.030 %
0.030 %
24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.011 cm/cm
0.011 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 47
47
ASTM D785
Hardness, Rockwell R 68
68
ASTM D785
Tensile Strength, Ultimate 21.4 MPa
3100 psi
ASTM D638
Elongation at Break >= 100 %
>= 100 %
ASTM D638
Flexural Strength 32.4 MPa
4700 psi
ASTM D790
Flexural Modulus 1.40 GPa
203 ksi
ASTM D790
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
ASTM D256
Izod Impact, Unnotched 9.60 J/cm
18.0 ft-lb/in
ASTM D256
Gardner Impact 11.3 J
8.33 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °C
129 °F
ASTM D648
Flammability, UL94 HB
HB