Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 318 MPa | 46100 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP PF00A PA 6 LNP THERMOCOMP* PF00A is a compound based on Nylon 6 resin containing 50% Glass Fiber. |
|||
Flexural Strength | 318 MPa | 46100 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP PF00A PA 6 (Asia Pacific) LNP THERMOCOMP* PF00A is a compound based on Nylon 6 resin containing Glass Fiber. |
|||
Flexural Strength | 318 MPa | 46100 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP PF00ASXS PA 6 LNP THERMOCOMP* PF00ASXS is a compound based on Nylon 6 resin containing 50% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Strength | 318 MPa | 46100 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP PF00ASXS PA 6 (Asia Pacific) LNP THERMOCOMP* PF00ASXS is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Strength | 318 MPa | 46100 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON RE0039 PA 66 LNP STAT-KON* RE0039 is a compound based on Nylon 66 resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Flexural Strength | 318 MPa | 46100 psi | ASTM D790 |
Ensinger Tecapeek® CF30 Polyetheretherketone, 30% Carbon Reinforced (PEEK) Tecapeek™, made from Victrex® PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance. Excellent .. |
|||
Flexural Strength | 318 MPa @Temperature 22.8 °C |
46100 psi @Temperature 73.0 °F |
ASTM D790 |
Ensinger Tecapeek® MT CF 30 Polyetheretherketone (PEEK) TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti.. |