Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 22.1 MPa | 3200 psi | ASTM D790 |
Quadrant EPP TIVAR® 1000 EC Electrically Conductive UHMW (ASTM Product Data Sheet) |
|||
Flexural Strength | 22.1 MPa | 3200 psi | ASTM D790 |
Quadrant EPP TIVAR® 88 UHMW-PE, Premium Glass Filled, Crosslinked Lining Material (ASTM Product Data Sheet) Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic fl.. |
|||
Flexural Strength | 22.1 MPa | 3200 psi | ASTM D790 |
Quadrant EPP Tivar® Premium UHMW-PE Tivar Premium UHMW-PE |
|||
Flexural Strength | 22.1 MPa | 3200 psi | ASTM D790 |
Fiberfil® PP-61/VO/NH Polypropylene Copolymer, Flame Retardant, non-halogenated, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 22.1 MPa | 3200 psi | Parallel |
Momentive Performance Materials BNC2 Boron Nitride (BN) Refractory Composite Boron Nitride is a unique engineering material. It is a soft, machinable ceramic which can be combined with other refractory ceramics including Aluminum Oxide, Silicon Nitride, Aluminum Nitride, Mu.. |
|||
Flexural Strength | 22.1 MPa | 3200 psi | ASTM D790 |
Techmer ES HiFill® PP 0475 Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 22.1 MPa | 3200 psi | |
UCAR Carbon UCAR® CS Extruded Graphite Densified prior to graphitization, Grade CS is an extruded graphite 25-30% higher in strength than CBY. Grade CS is a low ash graphite with an oxidation resistance similar to grade CBY. It is the ma.. |
|||
Flexural Strength | 22.1 MPa @Temperature 175 °C |
3210 psi @Temperature 347 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® A-1240 L Polyphthalamide (PPA)
(discontinued **) Amodel A-1240 L is a 40% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten.. |