Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 53.0 MPa @Strain 4.51 %, Temperature 150 °C |
7690 psi @Strain 4.51 %, Temperature 302 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® FR530 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont .. |
|||
Tensile Stress | 53.0 MPa @Strain 0.590 %, Temperature 0.000 °C |
7690 psi @Strain 0.590 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® FR70M30V0 NC010 Nylon 66
(Unverified Data**) 30% Mineral Reinforced Flame Retardant Polyamide 66 Zytel FR70M30V0 NC010 is a 30% mineral reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performa.. |
|||
Tensile Stress | 53.0 MPa @Strain 2.28 %, Temperature 90.0 °C |
7690 psi @Strain 2.28 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® EFE6053 BK413 Nylon 66
(Unverified Data**) 40% Mineral/Glass Reinforced Polyamide 66 Minlon EFE6053 BK413 is a 40% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance P.. |