Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 41.9 MPa @Strain 10.0 %, Temperature 150 °C |
6080 psi @Strain 10.0 %, Temperature 302 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 415HP NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 15% Glass Reinforced Polyethylene Terephthalate with Excellent Impact Resistance Rynite 415HP NC010 is a 15% glass reinforced modified polyethylene terephthalate improved for easy fast processing ov.. |
|||
Tensile Stress | 41.92 MPa @Strain 0.900 %, Temperature 100 °C |
6080 psi @Strain 0.900 %, Temperature 212 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS95G40DH1T BK261 Nylon
(Unverified Data**) Zytel® PLS95G40DH1T is a 40% GR impact modified PA, made with SHIELD technology, its superior heat & oil resistance combined with the "stone impact resistance" makes it ideal choice for use in seve.. |