Polymer Property : Tensile Stress = 2733 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 18.84 MPa

@Strain 13.03 %,
Temperature 90.0 °C
2733 psi

@Strain 13.03 %,
Temperature 194 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC1010 NC010 Nylon 1010  (Unverified Data**)
Unreinforced Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight. ..
Tensile Stress 18.84 MPa

@Strain 8.43 %,
Temperature 150 °C
2733 psi

@Strain 8.43 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 73M30 NC010 Nylon 6  (Unverified Data**)
30% Mineral Reinforced Polyamide 6 Minlon 73M30 NC010 is a 30% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro..