Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 1.70 MPa @Strain 100 % |
247 psi @Strain 100 % |
Flow; ISO 37 |
PolyOne OnFlex™ HT 50A-3S2099 Thermoplastic Elastomer (TPE) OnFlex™ HT thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds is specially formulated to deliver very good compression set performance at.. |
|||
Tensile Stress | 1.70 MPa @Strain 100 % |
247 psi @Strain 100 % |
ISO 37 |
PolyOne OnFlex™ S HF 60A-3S1982 Thermoplastic Elastomer (TPE) OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu.. |
|||
Tensile Stress | 1.70 MPa @Strain 100 % |
247 psi @Strain 100 % |
ISO 37 |
PolyOne OnFlex™ S KE 50A-3S1731 Thermoplastic Elastomer (TPE) OnFlex™-S KE thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to a variety p.. |
|||
Tensile Stress | 1.70 MPa @Strain 100 % |
247 psi @Strain 100 % |
ISO 37 |
PolyOne OnFlex™ S KG 50A-3S2017 Thermoplastic Elastomer (TPE) OnFlex™-S KG thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p.. |
|||
Tensile Stress | 1.70 MPa @Strain 100 % |
247 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® N8860 TPE, Nylon Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Auto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInformation from Alliance Polymers & Se.. |
|||
Tensile Stress | 1.70 MPa @Strain 300 %, Temperature 23.0 °C |
247 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7736-1 Thermoplastic Elastomer (TPE) Dynaflex™ G7736-1 is a general purpose compound designed to provide easy processing and a good surface finish. - Good Aesthetics - Good Ozone/UV Stability - High Flow for Thin-Wall Parts - Overmold.. |
|||
Tensile Stress | 1.70 MPa @Strain 6.03 %, Temperature 90.0 °C |
247 psi @Strain 6.03 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 1.70 MPa @Strain 0.0600 %, Temperature 23.0 °C |
247 psi @Strain 0.0600 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1000 BK385 Nylon 1010 UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight... |
|||
Tensile Stress | 1.70 MPa @Strain 5.00 %, Temperature 23.0 °C |
247 psi @Strain 5.00 %, Temperature 73.4 °F |
ASTM D638 |
DuPont Performance Polymers Hytrel® G3548L TPC-ET
(Unverified Data**) Hytrel® G3548L is a low modulus grade with nominal hardness of 35D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injec.. |