Polymer Property : Tensile Stress = 212 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 1.46 MPa

@Strain 100 %
212 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P2760 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 1.46 MPa

@Strain 0.160 %,
Temperature 90.0 °C
212 psi

@Strain 0.160 %,
Temperature 194 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6  (Unverified Data**)
Unreinforced Polyamide 6 Zytel 7335F NC010 is a nucleated lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 1.46 MPa

@Strain 0.0700 %,
Temperature 150 °C
212 psi

@Strain 0.0700 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 54G15HSLR BK031 Polyphthalamide (PPA)  (Unverified Data**)
15% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G15HSLR BK031 is a 15% glass reinforced toughened heat stabilized hydrolysis resistant high performance polyamide resin. It i..
Tensile Stress 1.46 MPa

@Strain 0.000 %,
Temperature 60.0 °C
212 psi

@Strain 0.000 %,
Temperature 140 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS90G30DR BK099 Nylon 66  (Unverified Data**)
Zytel® PLS90G30DR BK099 is a 30% glass reinforced PA66 nylon resin having superior resistance to hot engine coolant. It is particularly suitable for automotive Radiator End Tanks and other parts in..
Tensile Stress 1.46 MPa

@Strain 0.210 %,
Temperature 0.000 °C
212 psi

@Strain 0.210 %,
Temperature 32.0 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET  (Unverified Data**)
65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers
Tensile Stress 1.46 MPa

@Strain 18.09 %,
Temperature 200 °C
212 psi

@Strain 18.09 %,
Temperature 392 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET  (Unverified Data**)
65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers