Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 1.20 MPa @Strain 100 % |
174 psi @Strain 100 % |
ISO 37 |
PolyOne OnFlex™ S EF 40A-3S1964 Thermoplastic Elastomer (TPE) OnFlex™-S EF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver good mechanical properties together with excell.. |
|||
Tensile Stress | 1.20 MPa @Strain 100 % |
174 psi @Strain 100 % |
ISO 37 |
PolyOne OnFlex™ S EH 40A-3S7001 Thermoplastic Elastomer (TPE) OnFlex™ S EH thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver a great cost/performance ratio in addition to t.. |
|||
Tensile Stress | 1.20 MPa @Strain 100 % |
174 psi @Strain 100 % |
ISO 37 |
PolyOne OnFlex™ S KE 40A-3S1727 Thermoplastic Elastomer (TPE) OnFlex™-S KE thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to a variety p.. |
|||
Tensile Stress | 1.20 MPa @Strain 0.600 %, Temperature 150 °C |
174 psi @Strain 0.600 %, Temperature 302 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® BM6450XD BK560 Polybutylene Terephthalate (PBT)
(Unverified Data**)& Unreinforced Polybutylene Terephthalate Developed for Blow MoldingCrastin BM6450XD BK560 is an unreinforced supertough polybutylene terephthalate resin with very high viscosity for extrusion and blo.. |
|||
Tensile Stress | 1.20 MPa @Strain 5.00 % |
174 psi @Strain 5.00 % |
ISO 527-1/-2 |
DSM Arnitel® EL250 TPC-ET Injection Molding |
|||
Tensile Stress | >= 1.20 MPa @Strain 100 % |
>= 174 psi @Strain 100 % |
ISO 37 |
Austin Novel Materials Texalan® 365A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |
|||
Tensile Stress | >= 1.20 MPa @Strain 100 % |
>= 174 psi @Strain 100 % |
ISO 37 |
Austin Novel Materials Texalan® 665A Polyester and Polyether based TPU Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |