Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 93.92 MPa @Strain 0.900 %, Temperature 150 °C |
13620 psi @Strain 0.900 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® HTN 52G45HSL NC010 Polyphthalamide (PPA) Zytel® HTN52G45HSL NC010 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provide.. |
|||
Tensile Stress | 93.907 MPa @Strain 1.70 %, Temperature 0.000 °C |
13620 psi @Strain 1.70 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Sorona® 3015G NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& 15% Glass Reinforced Polytrimethylene Terephthalate with Resin Made from Bio-PDO Sorona 3015G NC010 is a 15% glass reinforced PTT resin containing 31% renewably sourced ingredients by weight (37% ba.. |
|||
Tensile Stress | 93.89 MPa @Strain 1.01022 %, Temperature 0.000 °C |
13620 psi @Strain 1.01022 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK615SF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for injecti.. |