Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 90.0 MPa @Strain 1.00 %, Temperature -30.0 °C |
13100 psi @Strain 1.00 %, Temperature -22.0 °F |
|
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 90.0 MPa @Strain 1.00 %, Temperature 0.000 °C |
13100 psi @Strain 1.00 %, Temperature 32.0 °F |
|
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 90.0 MPa @Strain 1.00 %, Temperature 23.0 °C |
13100 psi @Strain 1.00 %, Temperature 73.4 °F |
|
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 90.0 MPa @Strain 3.00 %, Temperature 100 °C |
13100 psi @Strain 3.00 %, Temperature 212 °F |
|
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 90.0 MPa @Strain 4.00 %, Temperature 120 °C |
13100 psi @Strain 4.00 %, Temperature 248 °F |
|
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 90.0 MPa @Strain 4.00 %, Temperature 80.0 °C |
13100 psi @Strain 4.00 %, Temperature 176 °F |
|
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, Conditioned Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 90.0 MPa @Strain 1.00 %, Temperature 0.000 °C |
13100 psi @Strain 1.00 %, Temperature 32.0 °F |
|
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, Conditioned Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 90.0 MPa @Strain 3.00 %, Temperature 120 °C |
13100 psi @Strain 3.00 %, Temperature 248 °F |
|
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 90.0 MPa @Strain 4.00 %, Temperature 150 °C |
13100 psi @Strain 4.00 %, Temperature 302 °F |
|
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 90.0 MPa @Strain 5.00 %, Temperature 150 °C |
13100 psi @Strain 5.00 %, Temperature 302 °F |
|
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 90.0 MPa @Strain 1.00 %, Temperature 23.0 °C |
13100 psi @Strain 1.00 %, Temperature 73.4 °F |
|
Solvay TECHNYL® A 218W V33 Natural T PA66, 33% glass fiber, DRY Description: TECHNYL® A 218W V33 Nat T is a polyamide 66, reinforced with 33% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The prod.. |
|||
Tensile Stress | 90.0 MPa @Strain 4.00 % |
13100 psi @Strain 4.00 % |
|
Solvay TECHNYL® A 221 PA66, DRY Description TECHNYL ® A 221 is an unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. It is available in natural colors. Benef.. |
|||
Tensile Stress | 90.0 MPa @Strain 4.00 % |
13100 psi @Strain 4.00 % |
|
Solvay TECHNYL® A 548B V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B V15 is a copolyamide 6.6/6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits:.. |
|||
Tensile Stress | 90.0 MPa @Strain 2.00 %, Temperature -40.0 °C |
13100 psi @Strain 2.00 %, Temperature -40.0 °F |
|
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th.. |
|||
Tensile Stress | 90.0 MPa @Strain 3.00 %, Temperature 23.0 °C |
13100 psi @Strain 3.00 %, Temperature 73.4 °F |
|
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th.. |
|||
Tensile Stress | 90.0 MPa @Strain 2.00 %, Temperature 120 °C |
13100 psi @Strain 2.00 %, Temperature 248 °F |
|
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, Conditioned Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due.. |
|||
Tensile Stress | 90.0 MPa @Strain 1.00 %, Temperature 80.0 °C |
13100 psi @Strain 1.00 %, Temperature 176 °F |
|
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, DRY Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due.. |
|||
Tensile Stress | 90.0 MPa @Strain 1.00 % |
13100 psi @Strain 1.00 % |
|
Solvay TECHNYLSTARâ„¢ S 60G1 V30 PA6, 30% glass filled, DRY Description: TECHNYLSTARâ„¢ S 60G1 V30 is a reinforced 30% GF organophosphorous flame retarded grade based on a patented high flow polyamide 6 resin (TechnylStar). This product is heat stabilized.. |
|||
Tensile Stress | 90.0 MPa @Strain 0.970 %, Temperature 23.0 °C |
13100 psi @Strain 0.970 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 530 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Polyethylene Terephthalate Rynite 530 NC010 is a 30% glass fiber reinforced modified polyethylene terephthalate resin with an outstanding balance of strength stiffness and tough.. |
|||
Tensile Stress | 90.0 MPa @Strain 1.73 %, Temperature -20.0 °C |
13100 psi @Strain 1.73 %, Temperature -4.00 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 79G13L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Toughened Polyamide 66 Zytel 79G13L NC010 is a 13% glass fiber reinforced toughened polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 90.0 MPa @Strain 6.00 %, Temperature 23.0 °C |
13100 psi @Strain 6.00 %, Temperature 73.4 °F |
ISO 527 |
BASF Ultrason E 3010 PES Ultrason E 3010 is an unfilled, higher viscosity injection molding and extrusion PES grade, tougher and with improved chemical resistance. |
|||
Tensile Stress | 90.0 MPa @Strain 6.00 %, Temperature -40.0 °C |
13100 psi @Strain 6.00 %, Temperature -40.0 °F |
ISO 527 |
BASF Ultradur B 4520 PBT Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade. |