Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 53.18 MPa @Strain 4.05 %, Temperature 150 °C |
7713 psi @Strain 4.05 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 80G33HS1L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G33HS1L NC010 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin with outstanding impact resistance developed usin.. |
|||
Tensile Stress | 53.18 MPa @Strain 4.52 %, Temperature -40.0 °C |
7713 psi @Strain 4.52 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® LC6200 BK385 Nylon 612
(Unverified Data**) Toughened Polyamide 612 Developed for ExtrusionInformation provided by DuPont Performance Polymers |