Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.80 MPa @Strain 100 %, Thickness 2.00 mm |
551 psi @Strain 100 %, Thickness 0.0787 in |
Type 1, 200 mm/min; Flow; DIN 53504 |
PolyOne OnFlex™ BIO 5370A-E0004 Thermoplastic Elastomer (TPE) OnFlex™-Bio 5300 series thermoplastic elastomer compounds are soft thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% of renewable materi.. |
|||
Tensile Stress | 3.80 MPa @Strain 100 % |
551 psi @Strain 100 % |
ISO 37 |
PolyOne OnFlex™ S FR 80A-3S1892 Thermoplastic Elastomer (TPE) OnFlex™-S FR thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially flame retarded with a highly effective, RoHS compliant halo.. |
|||
Tensile Stress | 3.80 MPa @Strain 100 % |
551 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® F7870 TPE, Fire Retardant Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Auto PartsSealsWire & Cable ElectronicsInformation from Alliance Polymers & Services, Distributor of Nantong Elastome.. |
|||
Tensile Stress | 3.80 MPa @Strain 5.85 %, Temperature 0.000 °C |
551 psi @Strain 5.85 %, Temperature 32.0 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process.. |
|||
Tensile Stress | 3.80 MPa @Strain 16.33 %, Temperature 160 °C |
551 psi @Strain 16.33 %, Temperature 320 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me.. |
|||
Tensile Stress | 3.80 MPa @Strain 71.13 %, Temperature 150 °C |
551 psi @Strain 71.13 %, Temperature 302 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 3.80 MPa @Strain 16.33 %, Temperature 160 °C |
551 psi @Strain 16.33 %, Temperature 320 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET 55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers |