Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.34 MPa @Strain 300 % |
484 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® C4960M TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Tensile Stress | 3.34 MPa @Strain 300 %, Temperature 23.0 °C |
484 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versollan™ OM 1262NX-1 Thermoplastic Elastomer (TPE) Versollan™ OM 1262NX-1 is a performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS and PC/ABS substrates. - Excellent Grip with Matte, Rubbery Finish - Proven Track R.. |
|||
Tensile Stress | 3.34 MPa @Strain 300 %, Temperature 23.0 °C |
484 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versollan™ OM 1262NX-9 Thermoplastic Elastomer (TPE) Versollan™ OM 1262NX-9 is a performance TPU alloy designed for thin-wall overmolding onto polycarbonate (PC), ABS, PC/ABS and copolyester substrates. - Excellent Grip with Matte, Rubbery Finish - P.. |
|||
Tensile Stress | 3.34 MPa @Strain 100 % |
484 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P1776 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 3.34 MPa @Strain 300 % |
484 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P1957TA TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 3.34 MPa @Strain 50.0 % |
485 psi @Strain 50.0 % |
Average; ASTM D412 Method A |
Seals Eastern 7352D Nano-PTFE Filled Fluoroelastomer Nano-PTFE filled fluoroelastomer for low wear in hot dynamic applicationsInformation provided by Seals Eastern. |
|||
Tensile Stress | 3.34 MPa @Strain 19.62 %, Temperature 90.0 °C |
484 psi @Strain 19.62 %, Temperature 194 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® G4078W TPC-ET
(Unverified Data**) Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject.. |
|||
Tensile Stress | 3.34 MPa @Strain 0.400 %, Temperature 150 °C |
484 psi @Strain 0.400 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 12T NC010 Nylon 66
(Unverified Data**) 36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T NC010 is a 36% mineral reinforced toughened heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performan.. |