Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.14 MPa @Strain 100 %, Temperature 23.0 °C |
310 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ 9570-1 Thermoplastic Elastomer (TPE) Versaflex™ 9570-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Tensile Stress | 2.14 MPa @Strain 100 %, Temperature 23.0 °C |
310 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ 9570-9 Thermoplastic Elastomer (TPE) Versaflex™ 9570-9 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Tensile Stress | 2.14 MPa @Strain 100 %, Temperature 23.0 °C |
310 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ OM 1060X-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 1060X-1 is an overmolding TPE with very good adhesion to PC or ABS-based plastics. - Good Surface Aesthetics - Rubbery Feel - Soft Touch - Very Good Bond to PC, ABS, PC/ABSColor conce.. |
|||
Tensile Stress | 2.14 MPa @Strain 100 %, Temperature 23.0 °C |
310 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ OM 1060X-9 Thermoplastic Elastomer (TPE) Versaflex™ OM 1060X-9 is an overmolding TPE with very good adhesion to PC or ABS-based plastics. - Excellent Bond to PC, ABS, PC/ABS - Good Surface Aesthetics - Rubbery Feel - Soft TouchPurge thoro.. |
|||
Tensile Stress | 2.14 MPa @Strain 300 %, Temperature 23.0 °C |
310 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ OM 9-802CL Thermoplastic Elastomer (TPE) Versaflex™ OM 9-802CL is a clear, soft touch TPE designed to bond to the following thermoplastics: PC, ABS, PC/ABS and copolyester. New Product. Commercial specifications have not been established... |
|||
Tensile Stress | 2.14 MPa @Strain 100 % |
310 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P2950T TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 2.14 MPa @Strain 300 % |
310 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P3845H TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 2.14 MPa @Strain 300 % |
310 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P3850H TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 2.14 MPa @Strain 100 %, Temperature 23.0 °C |
310 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7960-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7960-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Tensile Stress | 2.14 MPa @Strain 100 %, Temperature 23.0 °C |
310 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7960-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7960-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Tensile Stress | 2.14 MPa @Strain 100 %, Temperature 23.0 °C |
310 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7960-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7960-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Tensile Stress | 2.14 MPa @Strain 100 %, Temperature 23.0 °C |
310 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G2703-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2703-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance and a low coefficient of friction. - Adhesion to Polypropylen.. |
|||
Tensile Stress | 2.14 MPa @Strain 100 %, Temperature 23.0 °C |
310 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7660-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7660-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Tensile Stress | 2.14 MPa @Strain 100 %, Temperature 23.0 °C |
310 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7660-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7660-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Tensile Stress | 2.14 MPa @Strain 100 %, Temperature 23.0 °C |
310 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7960-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7960-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Tensile Stress | 2.14 MPa @Strain 300 % |
310 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Telcar® TL-1522B Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Stress | 2.14 MPa @Strain 100 % |
310 psi @Strain 100 % |
ASTM D412 |
Teknor Apex Telcar® TL-88-N873C BLK 111 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Stress | 2.14 MPa @Strain 97.14 %, Temperature 100 °C |
310 psi @Strain 97.14 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 3078 Polyester Elastomer TPC-ET
(Unverified Data**) 30 Shore D High Performance Polyester Elastomer with Non-discoloring Stabilizer Hytrel 3078 is a very low modulus grade with nominal hardness of 30D. It contains non-discoloring stabilizer. It can b.. |
|||
Tensile Stress | 2.14 MPa @Strain 97.14 %, Temperature 100 °C |
310 psi @Strain 97.14 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 3078FG Polyester Elastomer TPC-ET
(Unverified Data**) 30 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |