Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 1.72 MPa @Strain 300 % |
249 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P1760 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 1.72 MPa @Strain 100 %, Temperature 23.0 °C |
249 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7950-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7950-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Tensile Stress | 1.72 MPa @Strain 100 %, Temperature 23.0 °C |
249 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7950-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7950-1001-00 is an easy processing, general purpose material designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypro.. |
|||
Tensile Stress | 1.72 MPa @Strain 100 %, Temperature 23.0 °C |
249 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7950-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7950-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Tensile Stress | 1.72 MPa @Strain 100 %, Temperature 23.0 °C |
249 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7950-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7950-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Tensile Stress | 1.72 MPa @Strain 50.0 % |
249 psi @Strain 50.0 % |
Average; ASTM D412 Method A |
Seals Eastern 5753 Fluorocarbon-Elastomer Features:MIL-SpecFKM general serviceInformation provided by Seals Eastern. |
|||
Tensile Stress | 1.72 MPa @Strain 25.0 % |
250 psi @Strain 25.0 % |
ASTM D412 Method A |
Seals Eastern 7346 Extreme Low Temperature Service Rubber HNBR for cold temp (-50°C) and/or aqueous serviceInformation provided by Seals Eastern. |
|||
Tensile Stress | 1.72 MPa @Strain 1.02 %, Temperature 150 °C |
249 psi @Strain 1.02 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1010 NC010 Nylon 1010
(Unverified Data**) Unreinforced Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight. .. |