Polymer Property : Tensile Stress = 1.70 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 1.70 MPa

@Strain 100 %
247 psi

@Strain 100 %
Flow; ISO 37
PolyOne OnFlex™ HT 50A-3S2099 Thermoplastic Elastomer (TPE)
OnFlex™ HT thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds is specially formulated to deliver very good compression set performance at..
Tensile Stress 1.70 MPa

@Strain 100 %
247 psi

@Strain 100 %
ISO 37
PolyOne OnFlex™ S HF 60A-3S1982 Thermoplastic Elastomer (TPE)
OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu..
Tensile Stress 1.70 MPa

@Strain 100 %
247 psi

@Strain 100 %
ISO 37
PolyOne OnFlex™ S KE 50A-3S1731 Thermoplastic Elastomer (TPE)
OnFlex™-S KE thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to a variety p..
Tensile Stress 1.70 MPa

@Strain 100 %
247 psi

@Strain 100 %
ISO 37
PolyOne OnFlex™ S KG 50A-3S2017 Thermoplastic Elastomer (TPE)
OnFlex™-S KG thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p..
Tensile Stress 1.70 MPa

@Strain 100 %
247 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® N8860 TPE, Nylon Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Auto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInformation from Alliance Polymers & Se..
Tensile Stress 1.70 MPa

@Strain 300 %,
Temperature 23.0 °C
247 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7736-1 Thermoplastic Elastomer (TPE)
Dynaflex™ G7736-1 is a general purpose compound designed to provide easy processing and a good surface finish. - Good Aesthetics - Good Ozone/UV Stability - High Flow for Thin-Wall Parts - Overmold..
Tensile Stress 1.70 MPa

@Strain 6.03 %,
Temperature 90.0 °C
247 psi

@Strain 6.03 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 1.70 MPa

@Strain 0.0600 %,
Temperature 23.0 °C
247 psi

@Strain 0.0600 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC1000 BK385 Nylon 1010
UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight...
Tensile Stress 1.70 MPa

@Strain 5.00 %,
Temperature 23.0 °C
247 psi

@Strain 5.00 %,
Temperature 73.4 °F
ASTM D638
DuPont Performance Polymers Hytrel® G3548L TPC-ET  (Unverified Data**)
Hytrel® G3548L is a low modulus grade with nominal hardness of 35D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injec..