Polymer Property : Tensile Stress = 1.27 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 1.27 MPa

@Strain 100 %
184 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® C4740 TPE, Transparent
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf..
Tensile Stress 1.27 MPa

@Strain 100 %
184 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P2740 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 1.27 MPa

@Strain 100 %
184 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P1935 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 1.27 MPa

@Strain 7.29 %,
Temperature 60.0 °C
184 psi

@Strain 7.29 %,
Temperature 140 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 3078 Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D High Performance Polyester Elastomer with Non-discoloring Stabilizer Hytrel 3078 is a very low modulus grade with nominal hardness of 30D. It contains non-discoloring stabilizer. It can b..
Tensile Stress 1.27 MPa

@Strain 0.000 %,
Temperature 180 °C
184 psi

@Strain 0.000 %,
Temperature 356 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon  (Unverified Data**)
Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood..
Tensile Stress 1.27 MPa

@Strain 0.0700 %,
Temperature -40.0 °C
184 psi

@Strain 0.0700 %,
Temperature -40.0 °F
50%RH; ISO 11403-1/-2
DuPont Performance Polymers Zytel® RS LC1600 BK385 Nylon 1010  (Unverified Data**)
Zytel® RS LC1600 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced ingredient by weight. It is flexible, toughened, plasticized, UV and heat stabilized and s..
Tensile Stress 1.27 MPa

@Strain 7.29 %,
Temperature 60.0 °C
184 psi

@Strain 7.29 %,
Temperature 140 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 3078FG Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 1.27 MPa

@Strain 0.100 %,
Temperature -20.0 °C
184 psi

@Strain 0.100 %,
Temperature -4.00 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET  (Unverified Data**)
65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers