Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 1.24 MPa @Strain 100 %, Temperature 23.0 °C |
180 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ OM 1040X-1 Thermoplastic Elastomer (TPE) The Versaflex™ OM 1040X-1 is a medical compliant overmolding TPE with very good adhesion to PC or ABS-based plastics. - Good Surface Aesthetics - Rubbery Feel - Soft Touch - Very Good Bond to PC, A.. |
|||
Tensile Stress | 1.24 MPa @Strain 100 %, Temperature 23.0 °C |
180 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7940-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7940-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Tensile Stress | 1.24 MPa @Strain 100 %, Temperature 23.0 °C |
180 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7940-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7940-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion.. |
|||
Tensile Stress | 1.24 MPa @Strain 100 %, Temperature 23.0 °C |
180 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7940-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7940-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Tensile Stress | 1.24 MPa @Strain 100 %, Temperature 23.0 °C |
180 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7940-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7940-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion.. |
|||
Tensile Stress | 1.24 MPa @Strain 100 %, Temperature 23.0 °C |
180 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G2711-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2711-1000-00 is an easy process compound designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - O.. |
|||
Tensile Stress | 1.24 MPa @Strain 41.21 %, Temperature 120 °C |
180 psi @Strain 41.21 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 3078 Polyester Elastomer TPC-ET
(Unverified Data**) 30 Shore D High Performance Polyester Elastomer with Non-discoloring Stabilizer Hytrel 3078 is a very low modulus grade with nominal hardness of 30D. It contains non-discoloring stabilizer. It can b.. |
|||
Tensile Stress | 1.24 MPa @Strain 41.21 %, Temperature 120 °C |
180 psi @Strain 41.21 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 3078FG Polyester Elastomer TPC-ET
(Unverified Data**) 30 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |