Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 62.0 GPa @Temperature 25.0 °C |
8990 ksi @Temperature 77.0 °F |
|
Trelleborg AEM Eccospheres® FTD-200 Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Modulus of Elasticity | 62.0 GPa @Temperature 25.0 °C |
8990 ksi @Temperature 77.0 °F |
|
Trelleborg AEM Eccospheres® FTD-200 Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Modulus of Elasticity | 62.0 GPa @Temperature 25.0 °C |
8990 ksi @Temperature 77.0 °F |
|
Trelleborg AEM Eccospheres® FTD-250 Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Modulus of Elasticity | 62.0 GPa @Temperature 25.0 °C |
8990 ksi @Temperature 77.0 °F |
|
Trelleborg AEM Eccospheres® FTD-250 Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Modulus of Elasticity | 62.0 GPa @Temperature 25.0 °C |
8990 ksi @Temperature 77.0 °F |
|
Trelleborg AEM Eccospheres® IG-101 Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Modulus of Elasticity | 62.0 GPa @Temperature 25.0 °C |
8990 ksi @Temperature 77.0 °F |
|
Trelleborg AEM Eccospheres® SI-100 Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Modulus of Elasticity | 62.0 GPa @Temperature 25.0 °C |
8990 ksi @Temperature 77.0 °F |
|
Trelleborg AEM Eccospheres® SI-130 Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Modulus of Elasticity | 62.0 GPa @Temperature 25.0 °C |
8990 ksi @Temperature 77.0 °F |
|
Trelleborg AEM Eccospheres® SI-160 Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Modulus of Elasticity | 62.0 GPa @Temperature 25.0 °C |
8990 ksi @Temperature 77.0 °F |
|
Trelleborg AEM Eccospheres® SI-160 Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Modulus of Elasticity | 62.0 GPa @Temperature 25.0 °C |
8990 ksi @Temperature 77.0 °F |
|
Trelleborg AEM Eccospheres® SI-200 Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Modulus of Elasticity | 62.0 GPa @Temperature 25.0 °C |
8990 ksi @Temperature 77.0 °F |
|
Trelleborg AEM Eccospheres® SI-200 Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Modulus of Elasticity | 62.0 GPa @Temperature 25.0 °C |
8990 ksi @Temperature 77.0 °F |
|
Trelleborg AEM Eccospheres® SI-250 Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Modulus of Elasticity | 62.0 GPa @Temperature 25.0 °C |
8990 ksi @Temperature 77.0 °F |
|
Trelleborg AEM Eccospheres® SI-250 Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Modulus of Elasticity | 62.0 GPa @Temperature 25.0 °C |
8990 ksi @Temperature 77.0 °F |
|
Trelleborg AEM Eccospheres® SI-310 Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Modulus of Elasticity | 62.0 GPa @Temperature 25.0 °C |
8990 ksi @Temperature 77.0 °F |
|
Trelleborg AEM Eccospheres® SI-310 Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Modulus of Elasticity | 62.0 GPa @Temperature 25.0 °C |
8990 ksi @Temperature 77.0 °F |
|
Trelleborg AEM Eccospheres® SI-350 Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Modulus of Elasticity | 62.0 GPa @Temperature 25.0 °C |
8990 ksi @Temperature 77.0 °F |
|
Trelleborg AEM Eccospheres® SI-350 Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Modulus of Elasticity | 62.0 GPa @Temperature 25.0 °C |
8990 ksi @Temperature 77.0 °F |
|
Trelleborg AEM Eccospheres® SID-160Z Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Modulus of Elasticity | 62.0 GPa @Temperature 25.0 °C |
8990 ksi @Temperature 77.0 °F |
|
Trelleborg AEM Eccospheres® SID-160Z Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Modulus of Elasticity | 62.0 GPa @Temperature 25.0 °C |
8990 ksi @Temperature 77.0 °F |
|
Trelleborg AEM Eccospheres® SID-230Z Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Modulus of Elasticity | 62.0 GPa @Temperature 25.0 °C |
8990 ksi @Temperature 77.0 °F |
|
Trelleborg AEM Eccospheres® SID-230Z Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Modulus of Elasticity | 62.0 GPa @Temperature 25.0 °C |
8990 ksi @Temperature 77.0 °F |
|
Trelleborg AEM Eccospheres® SID-311Z Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Modulus of Elasticity | 62.0 GPa @Temperature 25.0 °C |
8990 ksi @Temperature 77.0 °F |
|
Trelleborg AEM Eccospheres® SID-311Z Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Modulus of Elasticity | 62.0 GPa @Temperature 25.0 °C |
8990 ksi @Temperature 77.0 °F |
|
Trelleborg AEM Eccospheres® SID-350Z Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Modulus of Elasticity | 62.0 GPa @Temperature 25.0 °C |
8990 ksi @Temperature 77.0 °F |
|
Trelleborg AEM Eccospheres® SID-350Z Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Modulus of Elasticity | 62.0 GPa @Temperature 25.0 °C |
8990 ksi @Temperature 77.0 °F |
|
Trelleborg AEM Eccospheres® W-25 Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Modulus of Elasticity | 62.0 GPa @Temperature 25.0 °C |
8990 ksi @Temperature 77.0 °F |
|
Trelleborg AEM Eccospheres® W-25 Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Modulus of Elasticity | 62.0 GPa @Temperature 25.0 °C |
8990 ksi @Temperature 77.0 °F |
|
Trelleborg AEM Eccospheres® W-30 Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Modulus of Elasticity | 62.0 GPa @Temperature 25.0 °C |
8990 ksi @Temperature 77.0 °F |
|
Trelleborg AEM Eccospheres® W-30 Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |
|||
Modulus of Elasticity | 62.0 GPa @Temperature 25.0 °C |
8990 ksi @Temperature 77.0 °F |
|
Trelleborg AEM Eccospheres® SID-120Z Sodium Borosilicate Glass Microspheres Eccospheres® glass microspheres are hollow thin-walled glass microspheres composed of sodium borosilicate glass. To the naked eye they resemble a fine, white, free-flowing powder. However, magnific.. |