Polymer Property : Modulus of Elasticity = 26000 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 179 GPa

@Temperature 649 °C
26000 ksi

@Temperature 1200 °F
Haynes R-41 alloy,
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
Modulus of Elasticity 179 GPa

@Temperature 649 °C
26000 ksi

@Temperature 1200 °F
Haynes R-41 alloy, 1.27 mm thick sheet, solution heat treated at 1079°C, water quenched, 30 minutes at 1066°C, air cooled, aged 16 hours at 760°C (1400°F)
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
Modulus of Elasticity 179 GPa

@Temperature 649 °C
26000 ksi

@Temperature 1200 °F
Haynes R-41 alloy, sheet 0.762-2.54 mm exclusive, 30 minutes at 1066°C, air cooled, aged 16 hours at 760°C (1400°F)
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
Modulus of Elasticity 179 GPa

@Temperature 649 °C
26000 ksi

@Temperature 1200 °F
Haynes R-41 alloy, sheet 0.762-2.54 mm exclusive, 30 minutes at 1121°C, air cooled, aged 16 hours at 899°C
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications includ..
Modulus of Elasticity 179 GPa

@Temperature 300 °C
26000 ksi

@Temperature 572 °F
Tension
Schmolz + Bickenbach UGIMA® 316/316L Stainless Steel Bar
Description: 316/316L UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 316L, except with respect to machinability. 316/316L UGIM..
Modulus of Elasticity 179 GPa

@Temperature 649 °C
26000 ksi

@Temperature 1200 °F
Haynes R-41 alloy,
Vacuum melted, exceptionally high strength at temperature between 649-982°C. Precipitation-hardening type, strength developed by various solutioning and aging heat treatments. Applications include ..