Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 4.40 GPa @Temperature 23.0 °C |
638 ksi @Temperature 73.4 °F |
MD; Test speed 1%/min.; 50% r.h.; ISO 527-1, ISO 527-3; Sample type 2 |
Mitsubishi Hostaphan® RN, 12 micron Nominal Thickness Universal Polyethylene Terephthalate Film Hostaphan® RN is a transparent, biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties. Hostaphan® RN is the standard product for.. |
|||
Modulus of Elasticity | 4.40 GPa @Temperature 23.0 °C |
638 ksi @Temperature 73.4 °F |
MD; Test speed 1%/min.; 50% r.h.; ISO 527-1, ISO 527-3; Sample type 2 |
Mitsubishi Hostaphan® RN, 15 micron Nominal Thickness Universal Polyethylene Terephthalate Film Hostaphan® RN is a transparent, biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties. Hostaphan® RN is the standard product for.. |
|||
Modulus of Elasticity | 4.40 GPa @Temperature 23.0 °C |
638 ksi @Temperature 73.4 °F |
MD; Test speed 1%/min.; 50% r.h.; ISO 527-1, ISO 527-3; Sample type 2 |
Mitsubishi Hostaphan® RN, 19 micron Nominal Thickness Universal Polyethylene Terephthalate Film Hostaphan® RN is a transparent, biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties. Hostaphan® RN is the standard product for.. |
|||
Modulus of Elasticity | 4.40 GPa @Temperature 23.0 °C |
638 ksi @Temperature 73.4 °F |
MD; Test speed 1%/min.; 50% r.h.; ISO 527-1, ISO 527-3; Sample type 2 |
Mitsubishi Hostaphan® RN, 23 micron Nominal Thickness Universal Polyethylene Terephthalate Film Hostaphan® RN is a transparent, biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties. Hostaphan® RN is the standard product for.. |
|||
Modulus of Elasticity | 4.40 GPa @Temperature 23.0 °C |
638 ksi @Temperature 73.4 °F |
MD; Test speed 1%/min.; 50% r.h.; ISO 527-1, ISO 527-3; Sample type 2 |
Mitsubishi Hostaphan® RN, 30 micron Nominal Thickness Universal Polyethylene Terephthalate Film Hostaphan® RN is a transparent, biaxially oriented film made of polyethylene terephthalate (PET) and characterized by outstanding physical properties. Hostaphan® RN is the standard product for.. |