Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 200 GPa @Temperature 300 °C |
29000 ksi @Temperature 572 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Bar, Hot Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Modulus of Elasticity | 200 GPa @Temperature 300 °C |
29000 ksi @Temperature 572 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Modulus of Elasticity | 200 GPa @Temperature 300 °C |
29000 ksi @Temperature 572 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Modulus of Elasticity | 200 GPa @Temperature 300 °C |
29000 ksi @Temperature 572 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Sheet, Cold Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Modulus of Elasticity | 200 GPa @Temperature 300 °C |
29000 ksi @Temperature 572 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Modulus of Elasticity | 200 GPa @Temperature 20.0 °C |
29000 ksi @Temperature 68.0 °F |
Tension |
Schmolz + Bickenbach UGIMA® 304 Cu Stainless Steel Bar Description: 304Cu UGIMA® is an enhanced machining grade produced only by Ugitech, providing the ultimate level of machinability available in an non-resulfurized austenitic stainless steel. 304Cu.. |
|||
Modulus of Elasticity | 200 GPa @Temperature 500 °C |
29000 ksi @Temperature 932 °F |
Tension |
Schmolz + Bickenbach UGIMA® 304 Cu Stainless Steel Bar Description: 304Cu UGIMA® is an enhanced machining grade produced only by Ugitech, providing the ultimate level of machinability available in an non-resulfurized austenitic stainless steel. 304Cu.. |
|||
Modulus of Elasticity | 200 GPa @Temperature 20.0 °C |
29000 ksi @Temperature 68.0 °F |
Tension |
Schmolz + Bickenbach UGIMA® 316/316L Stainless Steel Bar Description: 316/316L UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 316L, except with respect to machinability. 316/316L UGIM.. |
|||
Modulus of Elasticity | 200 GPa @Temperature 199 °C |
29000 ksi @Temperature 390 °F |
|
EDRO #3 Prehardened Mold Quality P20 Alloy Steel EDRO #3™ is a vacuum-degassed, ladle refined, Cr-Ni-Mo- alloyed steel which is supplied in the hardened and tempered condition. EDRO #3™ is manufactured to consistently high quality standards with.. |
|||
Modulus of Elasticity | 200 GPa @Temperature 20.0 °C |
29000 ksi @Temperature 68.0 °F |
|
EDRO EDRO400™ #40 Prehardened Insert Quality Martensitic Stainless Steel EDRO400™ is a remelted 400 series martensitic stainless steel supplied prehardened to 40 HRC (375 HB).EDRO400™ is characterized by excellent polishability, superior corrosion resistance, high leve.. |
|||
Modulus of Elasticity | 200 GPa @Temperature 20.0 °C |
29000 ksi @Temperature 68.0 °F |
|
EDRO RoyAlloy™ #6 Free Machining Stainless Holder Steel RoyAlloy™ is a 400 series martensitic stainless steel supplied prehardened. RoyAlloy™ is characterized by excellent machinability, good corrosion resistance, uniform and consistent hardness in all.. |
|||
Modulus of Elasticity | 200 GPa @Temperature 300 °C |
29000 ksi @Temperature 572 °F |
|
Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel BOHLER M303 EXTRA is a stainless martensitic chromium steel, offering excellent toughness, corrosion and wear resistance. It is characterized by improved machinability and polishability. BOHLER M303.. |
|||
Modulus of Elasticity | 200 GPa @Temperature 200 °C |
29000 ksi @Temperature 392 °F |
|
Bohler-Uddeholm UDDEHOLM MIRRAX ESR Plastic Mold Steel Uddeholm Mirrax ESR is specially developed and adapted for larger molds that require corrosion resistance and/or high surface finish.It is characterized by:High hardenability for consistent properti.. |
|||
Modulus of Elasticity | 200 GPa @Temperature 300 °C |
29000 ksi @Temperature 572 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Plate, Hot Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe.. |
|||
Modulus of Elasticity | 200 GPa @Temperature 300 °C |
29000 ksi @Temperature 572 °F |
Dynamic |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe.. |
|||
Modulus of Elasticity | 200 GPa @Temperature 20.0 °C |
29000 ksi @Temperature 68.0 °F |
Tension |
Schmolz + Bickenbach UGIMA 304/304L® Stainless Steel Bar Description: 304/304L UGIMA® is the next generation of improved high machinability grades from Ugitech. The UGIMA® grades have redefined high machinability stainless steels, showing improvements o.. |
|||
Modulus of Elasticity | 200 GPa @Temperature 100 °C |
29000 ksi @Temperature 212 °F |
Tension |
Schmolz + Bickenbach UGIMA 304/304L® Stainless Steel Bar Description: 304/304L UGIMA® is the next generation of improved high machinability grades from Ugitech. The UGIMA® grades have redefined high machinability stainless steels, showing improvements o.. |
|||
Modulus of Elasticity | 200 GPa @Temperature 200 °C |
29000 ksi @Temperature 392 °F |
Tension |
Schmolz + Bickenbach UGIMA 304/304L® Stainless Steel Bar Description: 304/304L UGIMA® is the next generation of improved high machinability grades from Ugitech. The UGIMA® grades have redefined high machinability stainless steels, showing improvements o.. |
|||
Modulus of Elasticity | 200 GPa @Temperature 300 °C |
29000 ksi @Temperature 572 °F |
Tension |
Schmolz + Bickenbach UGIMA 304/304L® Stainless Steel Bar Description: 304/304L UGIMA® is the next generation of improved high machinability grades from Ugitech. The UGIMA® grades have redefined high machinability stainless steels, showing improvements o.. |
|||
Modulus of Elasticity | 200 GPa @Temperature 400 °C |
29000 ksi @Temperature 752 °F |
Tension |
Schmolz + Bickenbach UGIMA 304/304L® Stainless Steel Bar Description: 304/304L UGIMA® is the next generation of improved high machinability grades from Ugitech. The UGIMA® grades have redefined high machinability stainless steels, showing improvements o.. |
|||
Modulus of Elasticity | 200 GPa @Temperature 500 °C |
29000 ksi @Temperature 932 °F |
Tension |
Schmolz + Bickenbach UGIMA 304/304L® Stainless Steel Bar Description: 304/304L UGIMA® is the next generation of improved high machinability grades from Ugitech. The UGIMA® grades have redefined high machinability stainless steels, showing improvements o.. |