Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 12.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
22.5 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Across Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 6935 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 12.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
22.5 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 85880 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 12.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
22.5 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87771 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 12.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
22.5 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L0189 Polyvinyl Chloride, Rigid (PVC, Rigid) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Izod Impact, Notched | 12.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
22.5 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L1101 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 12.0 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
22.5 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
notch |
Kraton® FG1901 + PBT blend (30/70), UV aged Carbon arc weatherometer UV aging for 360 hours. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A-B]n). The KRATON G series are second generation block polymers .. |
|||
Izod Impact, Notched | 12.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
22.5 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L5880 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 12.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
22.5 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L6181 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 12.0 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
22.5 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, all hinge breaks; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L6256 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |